Water ReducersPolycarboxylate Superplasticizer (Water-Reducing · Tablet)
97% solid content 0.1%–0.5% of total binder (as solid content)
Heat ResistantZJ-PC8310 is a powder polycarboxylate superplasticizer. Ultra-high water reduction, good plasticity retention, excellent heat resistance and good compatibility with gypsum systems. The product complies with GB 8076-2008 Concrete Admixtures and JG/T 223-2017 Polycarboxylate High-Performance Water Reducers and is suitable for cement- and gypsum-based building materials.
ZJ-PC8310 is a white to slightly yellow powder with pH 8.0±1.0, bulk density 600±100 g/L and moisture content ≤3.0%.
Simply blend the powder evenly into dry mixes before use; suitable for cement-based self-leveling mortars, grouts, anchor mortars, pressure grouting, UHPC, repair mortars, waterproof mortars and precast elements. Colour may vary from white to slightly yellow or yellow without affecting performance.
The following indicators are tested in accordance with GB 8076-2008 Concrete Admixtures and JG/T 223-2017 Polycarboxylate High-Performance Water Reducers.
| Item | Standard Requirement | Test Result |
|---|---|---|
| Appearance | White to slightly yellow powder | White to slightly yellow powder |
| Bulk density / (g/L) | 600±100 | 600±100 |
| Moisture content / % | ≤3.0 | ≤3.0 |
| pH value | 8.0±1.0 | 8.0±1.0 |
| Mortar water reduction / % | ≥25.0 | ≥25.0 |
For cement- and gypsum-based dry-mix mortars; different grades focus on self-leveling, grouting, UHPC and more.

Cement/gypsum self-leveling systems balancing flow retention and strength development.

Anchor mortars, pressure grouting and equipment-base grouting with excellent early strength and flow.

UHPC, repair and waterproof mortar systems.
Four steps to the best results, with our engineers assisting trial mixes and adjustments throughout.
Cement type, strength grade, slump requirement, transport distance and ambient temperature.
Engineers run 3–5 trial mixes for your conditions and issue a recommended dosage plan.
Small-batch verification at the plant, fine-tuning dosage to confirm workability and strength development.
Regular sampling and testing after supply starts, dynamically optimizing formulations for seasonal changes.
Water Reducers97% solid content 0.1%–0.5% of total binder (as solid content)
Water Reducers97% solid content 0.1%–0.5% of total binder (as solid content)
Water Reducers97% solid content 0.1%–0.5% of total binder (as solid content)
The recommended dosage is 0.8%–2.0% of binder weight, to be confirmed by trial mixes according to cement type, strength grade and temperature. Overdosing may cause segregation, bleeding or abnormal air content; follow the trial-mix dosage strictly and contact our technical service promptly if exceeded.
This product can be blended with naphthalene or aliphatic water reducers, air entrainers and retarders. However, compatibility tests must be run before blending products from different manufacturers — check for flocculation, precipitation or layering before use.
Store above 5 ℃. In cold weather, liquid products may thicken or crystallize — stir evenly and restore to room temperature before use without affecting performance. In winter concreting, avoid placing on frozen substrates and adjust curing measures accordingly.
Yes. We provide 5–20 kg free samples with trial-mix technical service for project customers. Fill in your project details in the inquiry form below and our engineer will contact you within 24 hours to arrange samples.
Fill in your project details and needs — our product engineer will contact you within 24 hours with quotation, samples and a trial-mix plan.